8. Solar Cells
8.1 General Concerns
8.1.1 Basic Solar Cell Topics
8.1.2 Solar Cell Current-Voltage Characteristics and Equivalent Circuit Diagram
8.1.3 Summary to: 8.1 Solar Cells - General Concerns
8.2 Making Bulk Si Solar Cells
8.2.1 Production Necessities and Silicon Starting Material
8.2.2 Processes and Process Integration
8.2.3 Summary to: 8.2 Making Bulk Si Solar Cells
8.3 Making Thin Film Solar Cells
8.3.1 Types of Thin Film Solar Cells
8.3.2 Essentials of Producing Thin Film Solar Cells
8.3.3 Summary to: 8.3 Making Thin Film Solar Cells
8.4 Summary
8.4.1 Summary to: 8 Solar Cells
© H. Föll (Semiconductor Technology - Script)