The Luristan Project - Literature Review | ||
|---|---|---|
| The actual review is a hodgepodge of comments in English or German, pictures and text quotes. often inserted as pictures. It is therefore in a Word format. | ||
| Here is the link. | ||
| The thre is a discussion of these papers in the context of our own results concnerning the "cut swowrd" in this link | ||
| The following papers are discussed. You can access them from here or from the Word document. | ||
| 1957 | F.
K. Naumann: Untersuchung eines eisernen luristanischen Kurzschwertes Archiv für das Eisenhüttenwesen, 28. Jahrgang, Heft 9, (1957) 575 - 581 | |
| 1961 | Herbert
Maryon; with technical reports by R. M. Organ, O. W. Ellis, R. M. Brick, R. Sneyers, E. E. Herzfeldand F. K. Naumann:
Early Near Eastern Steel Swords, American Journal of Archaeology, Vol. 65, No. 2 (Apr., 1961), pp. 173-184 |
|
| 1964 | Kate
C. Lefferts: Technical Notes on Another Luristan Iron Sword American Journal of Archaeology, Vol. 68, No. 1 (Jan., 1964), pp. 59-62 | |
| 1966 | K.
R. Maxwell-Hyslop and H. W. M. Hodges: Three Iron Swords from Luristan Iraq, Vol. 28, No. 2 (Autumn, 1966), pp. 164-176 | |
| 1968 | Vera
Bird and Henry Hodges: A METALLURGICAL EXAMINATION OF TWO EARLY IRON SWORDS FROM LURISTAN Studies in Conservation, 13 (1968), 215-223 215 | |
| 1971 | C.
S. Smith: The Techniques of the Luristan Smith Science and Archaeology (Ed. Rober H. Brill), Cambridge, Massachusetts, 1971 | |
| 1971 | P.
R. S. MOOREY: CATALOGUE OF THE ANCIENT PERSIAN BRONZES IN THE ASHMOLEAN MUSEUM The book is not available: the link leads to relevant parts of it | |
| 1973 | E.
Schumacher: Eisenschwerter mit Maskenzier aus Luristan Kleemann Festschrift II Teil (=Bonner Hefte zur Vorgeschichte, n. 4), Bonn, 1973, p-97 ff | |
| 1987 | Claude
Forrieres, Étude par microscopie électronique de structures de trempe d'une lame d'épée
du Luristan, Étude par microscopie électronique de structures de trempe d'une lame d'épée du
Luristan ArchéoSciences, revue d'Archéométrie Année 1987 11 pp. 17-29 |
|
| 1988 | O.
Muscarella: "Bronze and Iron", (Book) New York 1988 (pp 184 . 189) |
|
| 1991 | J. E. Rehder, The Decorated Iron Swords From Luristan: There Material And Manufacture; Journal of Persian Studies, Iran, Vol. 29 (1991) pp. 13 - 19 | |
| 1991 | P.R.S. Moorey The Decorated Ironwork of the Early Iron Age Attributed to Luristan in Western Iran | |
| 2003 | Bruno
Overlaet, The Early Iron Age in the Pusht-i Kuh; Luristan; Acta Iranica, Vol. XXVI, 2003; selected parts of the huge volume | |
| 2003 | FRANCE-LANORD, A.:1969 La Fer en Iran au premier millenaire avant Jesus Christ. Revue d'histoire des mines and metallurgie I, 75-126. Probably important paper but can't get a copy |
|
| 2005 |
Bruno Overlaet, The Chronology of the Iron Age in the Pusht-i Kuh Luristan, Iranica Antiqua, Vol XL (2005), pp. 1 - 33 | |
| 2009 | Moshtagh Khorasani, Manouchehr, Bronze and iron weapons from Luristan | |
| 2015 | A.
Hasanpur et al.; The Baba Jilan Graveyard Near Nurabad, Pisht-i Kuh, Luristan - A Preliminary Report, Iranica Antiqua, Vol. L (2015), pp 171 -212 | |
Discussion of the "Cut Sword" Findings
Part 1 Basics about Scythians and Their Akinakai
First Iron Swords - Double-Disc Hilt Sword
The Luristan Project - Results from Cut Swords
Literature to "Scythian Special"
© H. Föll (Iron, Steel and Swords script)