Part 1: Basics about Scythians and their Akinakai | ||
| The Starting Point | ||
| Iron and steel technology developed slowly and was limited for quite some time to relatively simple objects that were extremely precious. King Tut's iron dagger from around 1330 BC may be seen as the high point of this early technology. Complex iron / steel objects, like the Luristan mask swords or Celtic "Hallstatt" swords, appeared "suddenly" around 900 BC all over the place, it seems. Exact dates are very difficult to come by, however, and not many studies into the evolution of complex iron products have been made. | ||
| As pointed out in the the module accessible by the link given above, the major
objects one could study are the Luristan iron swords (type 1 and 2),
the early Celtic / Hallstatt swords, sundry swords from here, there
and then - and, possibly, early akinakai and in particular early Scythian akinakai
1). Why? Because they are around in relatively large numbers; easily acquired from one of the many auctions houses dealing with antiquities. We thus could spare a few for "destructive" in-depth metallurgical studies. | ||
| Scythian akinakai are easily distinguished
from the general type since they have a guard of the "bollocks"
type; examples can be seen here. I use the somewhat indelicate word conscientiously
since the old Scythians were proud of that part of their anatomy as demonstrated by one of their big chieftains here. Scythian akinakai also do not have elaborately decorated hilts for showing off but project rather power, prowess and violence; in contrast to other akinakai around in 800 - 600 BC. What I'm trying to here is to look at Scythians and their akinakai in the context of who else was around after, say, 800 BC with a sufficiently powerful iron technology. Did other powers / cultures / empires and so one produce or use bollocks types of akinakai? |
||
Questions that come up in this context are:
| ||
| Nothing helps. We need to get a grip on "The Scythians and their bollocks
akinakai" plus their relations to other folks around then and there, like the Assyrians, Medians, Cimmerians, Dacians,
Persians, Greeks, etc.) who definitely used weapons and might have produced weapons similar to Scythian akinakai. At this point a scientist like me needs to study the literature in order to find out what is already known about the technology used for making all kinds of Akinakai. | ||
| Well, that turned out to be easy: Next to nothing is known about the metallurgy of akinakai
and thus also next to nothing is known about the technology used. More to that in the "Akinakai"
module On a positive note, we do have a kind of dating system for akinakai that allows to make educated guesses at the age of the akinakai around in museums and private collections. That motivated me to take a closer a look at some akinakai and to start this special "Scythian Akinakai" module. At the time I'm writing this (March 2020), I have no idea to where this will lead to but I hope that some new information will become available. |
||
| In this module I now look at some basics about the Scythians and their possibly akinakai making and wielding contemporaries | ||
| Scythians - Some Basics | |||||
| You can't do much better than Wikipedia for a concise but still detailed description of Scythians. In what follows I use mainly Wikipedia texts but shorten or embellish them here and there. | |||||
| "The Scythians were a nomadic
people who dominated Pontic steppe from about the 7th century BC up until
the 3rd century BC. They were part of the wider Scythian cultures, stretching across the Eurasian Steppe, which included
many peoples that are distinguished from the Scythians. Because of this, a broad concept
referring to all early Eurasian nomads as "Scythians" has sometimes been used. Within this concept, the actual Scythians (=wielders of the bollocks type of akinakai?) are
variously referred to as Classical Scythians, European Scythians, Pontic Scythians, or Western Scythians. The Scythians are generally believed to have been of Iranian origin. They spoke a language of the Scythian branch of the Eastern Iranian languages, and practiced a variant of ancient Iranian religion. Among the earliest peoples to master mounted warfare, the Scythians replaced the Cimmerians as the dominant power on the Pontic Steppe in the 8th century BC. During this time they and related peoples came to dominate the entire Eurasian Steppe from the Carpathian Mountains in the west to Ordos Plateau in the east, creating what has been called the first Central Asian nomadic empire. Based in what is modern-day Ukraine and southern Russia, the Scythians were led by a nomadic warrior aristocracy known as the Royal Scythians, who called themselves Scoloti In the 7th century BC, the Scythians crossed the Caucasus and frequently raided the Middle East along with the Cimmerians , playing an important role in the political developments of the region. Around 650–630 BC, Scythians briefly dominated the Medes of the western Iranian Plateau, stretching their power to the borders of Egypt. After losing control over Media, the Scythians continued intervening in Middle Eastern affairs, playing a leading role in the destruction of the Assyrian Empire in the Sack of Nineveh in 612 BC. The Scythians subsequently engaged in frequent conflicts with the Achaemenid Empire. The Scythians suffered a major defeat against Macedonia in the 4th century BC and were subsequently gradually conquered by the Sarmatians, a related Iranian people living to their east." I stop here because we are not much interested into anything after about 500 BC. Now let's look at some of the catch words from above | |||||
| Nomadic People. The Scythians of whatever
specific domination were actually "Reiternomaden
", meaning horse-based nomads, i.e. people without a permanent place for living who moved around on horseback.
There seems to be no good English word for that; you see once more the advantage of using the true
language . Horses were domesticated (as far as we know) somewhere in the Eurasian Steppes approximately 3500 BC. The Scythians moving around the Pontic steppe (and beyond) in the 7th century BC and later thus had plenty of time to become experienced horse breeders and riders, feared by all and sundry that did not have an effective cavalry of there own. Their main weapon was the composite recurve bow, allowing powerful shots from horse back. The Romans (and may others) were quite impressed. Nobody was impressed by their akinakai, which were of course, rather useless while on horseback. | |||||
| |||||
| Actual Scythians wielding a bollocks type of akinakai may have been around all over the place too, but here we concentrate on those that have settled down (up to a point) in the Crimea and North of the Black Sea (see above and below). Their akinakai have a very typical guard of the bollocks type. If you use this link you can see why this term is quite precise, if a bit vulgar. | |||||
| A very learned and long paper about the Scythians is provided by the "Encyclopædia
Iranica". Refer to it for all details and in particular if you are interested in the writings of Herodotus and
others about these folks. Unfortunately, we learn very little about Scythian metal technology. Now let's give a quick look to the Scythian culture. Once more, via Wikipedia. |
|||||
| "The Scythian cultures are characterized by the Scythian
triad, which are similar, yet not identical, styles of weapons, horses' bridles and Scythian art. The question of how related
these cultures were is disputed among scholars. Its peoples were of diverse origins, and included not just Scythians, from
which the cultures are named, but other peoples as well, such as the Cimmerians
, Massagetae, Saka, Sarmatians and obscure forest steppe populations. Mostly speakers of the Scythian branch of the
Iranian languages, all of these peoples are sometimes collectively referred to as Scythians. " "The Scythian culture flourished across the entire Eurasian Steppe during the Iron Age from approximately the 9th century BC to the 2nd century AD" "Recent excavations at Arzhan in Tuva, Russia have uncovered the earliest (around 800 BC) Scythian-style things found so far" | |||||
| Here are the early Scythian-style daggers or akinakai that were found among those things | |||||
| |||||
| The Arzan "kurgan" (=tell=burial mound or hill) is several 1000 km to the east of the Crimea, the center of the Scythians area after they settled (as far as horse people settle) there around 700 BC or so. What we see is also not quite the typical "bollocks" type of Scythian akinaka. It would be interesting to learn something about the metallurgy of these weapons but (of course) no investigation has been made. | |||||
| In short: Wherever and whenever the Scythian culture evolved might be open to discussion but is not of much interest to us here. We simply lack iron objects from this early time. The akinakai we could investigate originated most likely from an area north of the Black Sea as shown below: | |||||
| |||||
|
All the other kinds of akinakai shown here in a roughly chronological
order were also found in this general area (which includes present day Turkey, Bulgaria; Rumania, Moldova, Ukraine, Russia,
Georgia and Armenia). The oldest ones date from the 7th - early 6th century, i.e. from roughly 700 - 570 BC. That does not imply that akinakai weren't also found outside the region shown above, e.g. in present day Hungary or even Poland. The Hungarian National Museum in Budapest shows a nice one from around 650 BC, for example. There are older akinakai too (like the ones shown above) but they seem to be rare and certainly not available for a metallurgical examination. If there are much older akinakai of the bollocks type I don't know. |
|||||
| If you want to know more about the Scythians around the Black Sea, read the Article
in the Encyclopædia
Iranica. In the remainder of this module we take a quick look at other cultures next to the Scythians in time and place.
This will help to appreciate what makes the Scythians Akinakai so special. To some extent this will overlap with what I have written here and there - but so what. | |||||
Other Folks | ||||||||
| Background | ||||||||
| Next we take a quick look at the other folks around during the early Scythian period, i.e. during 7th - early 6th century and what kind of akinaka, if any, they carried. What we encounter, according to Wikipedia (plus additions in red by me) , is: | ||||||||
| ||||||||
| We may just about forget about the Kingdom of Israel and the Kingdom of Judah. They were of no importance and come up only because the old guys there heeded the first law of scientific success: publish or perish and produced (parts of) what later became known as "bible". The Neo-Assyrians also left a lot of (cuneiform) writing - in contrast to, e.g., the Luristanis and Scythians, who left heavy metal. | ||||||||
It is also helpful to look at a list of major happenings in the beginning of the
first millennium (from Wiki, of course; except for lines 9. and 10.):
|
||||||||
| I'm going to skip the early Jews and the Egyptians because they have (as far as I'm aware of) nothing to offer in terms of iron technology. Contrariwise, I have emphasized the enterprises of Sargon II because his 160 tons of iron found in his (short-lived) capital in Khorsabad make a kind of strong statement. | ||||||||
| We might actually take this iron as a focal point for this module. Why did Sargon
hoard 160 tons of iron in the form of double-pyramid bars, the result of about 16.000 iron smelting runs? Just to be prepared
for bad times? Or did he actually take it from the extremely rich kingdom of Carchemish (line 10. above)? Wikipedia reports:
"This conquest allowed Sargon to secure Pisiri's large treasury, including 330 kilograms of purified
gold, large amounts of bronze, tin, ivory and iron and over 60 tonnes of silver"" In any case, we may assume that the double-pyramid bar was the starting material for most iron products in the general area around 700 BC and probably for many years before and after. Most if not all early akinakai were probably made from this kid of iron. | ||||||||
| We now need to look at the Assyrians and (neo) Babylonians | ||||||||
| Assyrians and Babylonians | ||||||||
| We start with line 2. from above: "884 to 858 BC – Ashurnasirpal II, king of Assyria , embarked on a vast program of expansion...". We have the start of the Assyrian empire. 279 years later (605 BC) it will be overtaken be the Neo-Babylonian empire. There is not much I can say here that I haven't said before. We seem to know next to nothing about the "iron" of these empires as stated here. Well, not quite true. Iron s imentioned ever so oftne in in written material and we have some iron artifacts. More to that in the paper of Caroline van der Brugge.. Maps and some information about these empires you will find in this link. However, we need to remember once more that Sargon II not only built "Dur-Sharrukin" (meaning "Fortress of Sargon"; present day Khorsabad) but had a stockpile of 160 tons of iron there, roughly 20.000 double pyramid bars. You needed 15.000 - 30.000 smelting runs for producing that much iron. It appears to be a lot of iron but it is just about enough to fully equip 20.000 - 30.000 soldiers and their entourage with weapons and supporting stuff. We must conclude that the Assyrians (and therefore also the Neo-Babylonians who took over later) were running a sizeable iron industry after, roughly, 750 BC. We just don't have any products. | ||||||||
| However, looking at various stelae, friezes and sculptures of Assyrians, we see swords and daggers but no bollock types akinakai. Examples follow. | ||||||||
| ||||||||
| Ashurnasirpal is fingering his "typical" Assyrian sword (no good one
was ever found, bur look here) and at least
two daggers that are definitely not of the bollocks akinaka type. Here is Sargom II: |
||||||||
| ||||||||
| ||||||||
| Saron II was the Assyrian King from 722 BC - 705 BC. Royal fashion has not changed much since Ashurnasirpal but Sargon no longer burdens himself with daggers. Similar kind of sword, though. Note that his sword has what I called a winged chape, hinting at cavalry use, like the (rather long) sword of Ashurnasirpal II (ca. 883-859 B.C.) shown here. | ||||||||
| Sargon II was the one who in 713 BC began the construction of Dur-Sharrukin
(present day Khorsabad) as his new capital. He noved in in 706 BC and out (by being killed in battle) a year later (705
BC). After his death the city was abandoned - with the 160 tons of iron left back! Obviously it was not all that precious.
Sargon's successors (Sennacherib, 705–681, Esarhaddon, 681–669 BC, Ashurbanipal, 668–631 BC and so on) kept the empire going for another 100 years or so until the final (bloody) end in 609 |
||||||||
| Starting 612 BC we now have the Neo-Babylonian empire also known as Chaldean empire. It started more or less with King Nebuchadnezzar II of Babylon causing a lot of grief to early Jews (destruction of Solomon's Temple in Jerusalem in 687 BC, deportation of the Jews to Babylon in 597 BCE, 587/586 BCE, and 582/581 BC respectively). That resulted in a lot of bad press for Nebuchadnezzar and the Babylonians, with topics like the building of the tower of Babel followed inciting some God confounding speech, or the ever popular whore of Babylon. | ||||||||
| However, the Jews doing time in Babylon failed to write down something about
Babylonian iron technology. So did everybody else (failing to write down something about iron technology and its products)
and as a result we seem to know exactly nothing about this topic. It doesn't matter much, however, because the Neo-Babylonians came too late to be of much interest anymore. The obviously were an aggressive bunch given to warfare and thus must have had all kinds of iron / steel weapons. But in 600 BC iron technology was well established in Mesopotamia and elsewhere. That doesn't mean that we know much about this but we can't expect big surprises anymore if we ever get around to analyzing the little we have. | ||||||||
| How did the Scythians relate to the Assyrians? In many ways, says Wikipedia: "In the 670s, the Scythians under their king Bartatua raided the territories of the Assyrian Empire. The Assyrian king Esarhaddon managed to make peace with the Scythians by paying a large amount of tribute." Did the tribute, perhaps, include iron and iron products like akinakai? "Bartatua was succeeded by his son Madius ca. 645 BC, after which they (i.e. the Scythians) launched a great raid on Palestine and Egypt . Madius subsequently subjugated the Median Empire. During this time, Herodotus notes that the Scythians raided and exacted tribute from "the whole of Asia". That is just anther way of saying that the Scythians had access to whatever iron technology was around then. "In the 620s, Cyaxares, leader of the Medes, treacherously killed a large number of Scythian chieftains at a feast; the Scythians were subsequently driven back to the steppe. In 612 BC, the Medes and Scythians participated in the destruction of the Assyrian Empire with the Battle of Nineveh. During this period of influence in the Middle East, the Scythians became heavily influenced by the local civilizations". |
||||||||
| Maybe the Scythians made their own bollocks akinakai, maybe somebody else was persuaded to make them for them. In either case,. given the constant loving or not-so-loving interaction of everybody down there with everybody else, we may be safe in assuming that the bollocks akinakai mirror the general status of iron / steel technology in the area. | ||||||||
| Early Greece | ||
| Point 4 is next: 800 to 480 BC – Archaic period in Greece
with the rise of the city-states, Greek colonies, and Epic Greek poetry. Not to mention the first Olympic Games in 776 BC.
We know that the ancient Greeks were good fighters with several kinds of sword types; refer to this link. We have the xiphos , makheira and the kopis / falcata - and most of what he have was made from bronze. | ||
| What I can say about Greek iron technology here is exactly the same as what I have said in the link above: Nothing! I know nothing about Greek iron, and I have no idea if the old Greeks ever fashioned something like a (bollocks) akinaka. | ||
| I know, however, (e.g. form Wikipedia) that the Scythians and the early Greeks
interacted quite a bit: "In the 6th century BC, the Greeks had begun establishing settlements along the coasts and rivers of the Pontic steppe, coming in contact with the Scythians. Relations between the Greeks and the Scythians appear to have been peaceful, with the Scythians being substantially influenced by the Greeks". True enough, just look at the famous "Scythian gold" that shows heavy Greek influence. |
||
| Elam, Median Empire, and the Persian Achaemenid Empire | |||||||||
| Elam and the Median Empire lead up to the Achaemenid Empire and merit a few notes. Elam existed for a long time and was somehow connected to Luristan, the Jiroft culture and many others. It left us breathtakingly beautiful silver objects. | |||||||||
| It did not leave us any iron artifacts however, not to mention swords or daggers. On occasion bronze daggers usually associated with Luristan are claimed to be Elamite but nothing is coming close to a bollocks akinaka. | |||||||||
| Same thing for the Median empire except that they did not last very long (see below) and left not many metal artifacts at all, certainly no iron daggers of any kind. | |||||||||
| However, some of the guys shown in Persian friezes and stelae are Median warriors
and they do carry something coming rather close to a bollocks akinaka (see way below), in contrast to the Persian guys sporting
daggers that were definitely not of the bollocks type but rather of the "elaborate show-off hilt" type. But by
then the Medians were already subdued by the Persians and that lead us right to the Achaemenid empire. For starters let's look at some maps showing what was going on in the Iranian core region between 678 BC and 547 BC: |
|||||||||
| |||||||||
| Persia - Achaemenid Empire | |||||
| The way present day Iran feels about Iranians around 500 BC is neatly shown in the map below: | |||||
| |||||
| Most about everybody who was somebody was some kind of Iranian, certainly the
Scythians, Sarmatians, plus whoever lived in Mesopotamia, Turkey, Egypt, Arabia, etc. Just the "Greek City States", Thrace, Illyria and Etruscans / Romans are acknowledged as independent powers with some vague pretense to culture besides the sundry barbarians far away. Seems a bit strange but may not have been all that wrong. However, we look in particular at the time horizon 700 BC - 600 BC and then we still had the Babylonian, Assyrians, etc. as major powers, see below or here. | |||||
| Anyway - what do we know about the "Iranian" daggers / swords from around 700 BC - 500 BC? | |||||
| Easy. A look into Khoransani's
wonderful book "Arms and Armor from Iran"
shows two things: 1. Most "old" stuff (mostly bronze) is from Luristan, the link shows plenty of examples. 2. There seems to be nothing there that looks even remotely like a "Scythian" akinaka.. Well, we also have stelaes, friezes and sculptures of old Iranians wearing weapons, like these guys: |
|||||
| |||||
| Persepolis was the ceremonial capital of the Achaemenid Empire (ca. 550–330 BC), built (most likely) by Darius the Great. What we see above
for the Persian guys does not look like the handles of Scythian "bollocks" types akinakai. Other
daggers found on friezes might come closer to akinakai but they might be worn by members of other cultures like the
Medians as stated before. It is also of some interest that the peculiar kind of scabbard or sheath we find on those friezes does have close relation to some known from Scythians: | |||||
| |||||
| I cannot imagine that huge empires like the Achaemenide empire had a metal technology that was inferior to that of the Scythians. Maybe the Scythians bought their akinakai from the Assyrians / Greeks / Iranians and so on, or just imported the know-how. They did take over a lot of Greek things (for example in their gold) art) after all. | |||||
| Cimmerians and Urartu | |||||
| The Cimmerians were only mentioned once in line 19 in the list above but have
much older relations to the Scythians as Wikipedia knows: "The Cimmerians were a nomadic Indo-European people, who appeared about 1000 BC and are mentioned later in 8th century BC in Assyrian records. While the Cimmerians were often described by contemporaries as culturally "Scythian", they evidently differed ethnically from the Scythians proper, who also displaced and replaced the Cimmerians. Probably originating in the Pontic steppe, the Cimmerians subsequently migrated both into Western Europe and to the south, by way of the Caucasus. Some of them likely comprised a force that, c. 714 BC, invaded Urartu, a state subject to the Neo-Assyrian Empire. This foray was defeated by Assyrian forces under Sargon II in 705, after which the same, southern branch of Cimmerians turned west towards Anatolia and conquered Phrygia in 696/5. They reached the height of their power in 652 after taking Sardis, the capital of Lydia; however an invasion of Assyrian-controlled Anshan was thwarted. Soon after 619, Alyattes of Lydia defeated them. There are no further mentions of them in historical sources, but it is likely that they settled in Cappadocia." Nomadic, from the Ponitic stepper, etc. They also were prominent during Sargon's the iron hoarder's rule and beyond:
|
|||||
| Busy guys with probably good weapons, not to mention bollocks. What do we know about that? Not much but we do have a few pictures: | |||||
| |||||
| |||||
| Not the typical Scythian bollocks type of akinaka, but not so different from the early Scythians ones from Arzhan kurgan. | |||||
| Now what about Urartu
? "Urartu is a geographical region commonly used as the exonym for the Iron Age kingdom also
known by the modern rendition of its endonym, the Kingdom of Van, centered around Lake
Van in the historic Armenian Highlands (present-day eastern Anatolia). The kingdom rose
to power in the mid-9th century BC, but went into gradual decline and was eventually
conquered by the Iranian Medes in the early 6th century BC." says Wikipedia.
Some contact to the Scythians occurred but Urartu is hardly worthwhile to mention here - except for the fact that I have in my possession more pictures of Urartu daggers or short swords than what you find in the Net: |
|||||
| |||||
| The only picture in the Net is from a professional firm (Alamy) that wants money.
Their picture shows the two swords on the right; it also supplies the German text inserted in the picture above. One thing is certain. These (bronze) weapons may or may not be are from Urartu but they definitely are not bollocks akinakai. We thus can forget about Urartu. It may or may not have played a role in the development of early iron technology (as manifested in Bollocks type of akinakai) - we just don't know. | |||||
| Dacians and Thracians | |||||
| These people figure heavily in Roman history and before in Greek history. They
populated the area around and west of the Danube estuary, i.e. present day Bulgaria and Rumania since 800 BC or longer. While the Internet does produces "Dacian akinakai" on occasion, their known weapons were quite different. They wielded the (short) sica and the (longer) falx , inward curving blades of the yatagan type, similar to the fkopis / alcata known from ancient Greek. See the paper of A. Rustoiu about Thracian weapons for detais | |||||
| Of course we don't seem to know a thing about their early metal technology, so let's forget them at this point. | |||||
| |||||
| Conclusion | ||||
| Bollock type akinakai were made by smiths who had access to suitable raw iron and some technology. It is quite possible that these smiths were Scythians but it cannot be ruled out that these daggers were made by some of the other cultures around the Scythians. We don't know but it hardly matters. Given the constant belligerent or peaceful mixing of people and cultures during the time period in question, basic technologies and materials must have been accessible by all and sundry most of the time. | ||||
| That implies that whatever iron product from a given time horizon you analyze,
it will point to the same general technology, no matter if it originally belonged to a Scythian, Assyrian,. Median, or whoever.
It will only point tot the general technology since ancient smiths, as we know from analyzing for example, Celtic swords, worked within a large bandwidth of capabilities, local customs, and statistical
fluctuations of, e.g. iron quality. What that means is obvious: | ||||
| ||||
| Let's do it! There are enough expendable iron akinakai around to "sacrifice" a few. It is not a real sacrifice anyway since the leftovers are still of large interest, witness the Luristan cut-sword project | ||||
| 1) | Grammar: It's one akinaka or akinakes and many akinakai or akinakes. |
Early Metal Technology - 2. Silver and Lead
Part 1 Basics about Scythians and Their Akinakai
Critical Museum Guide: Museums in Istanbul, Turkey
11.1.4 Swords of Major Near East Powers in the 1st Millennium BC
Scythian Special Large Pictures
Early Iron Making Empires in the Middle East / Mediterranean
First Iron Swords - Miscellaneous Objects
The Luristan Project - Results from Cut Swords