11.1.4 Swords of Major Near East Powers in the 1st Millennium BC | ||
| What's It About | ||
| You know that I'm not an expert for swords. I do know a thing or two about semiconductors,
and I also know something about the Materials Science and Engineering of metals. I know a sword if I see one and I have
some idea about how it is made and what - mechanically - it can do. But I did not know about akinakai
(singular is akinaka or akinaces), for example, until I had finished the preceding module and found out about these things
more or less by accident. I also just recently run across the Moroccan Nimcha sabre. I'm sure I don't know a lot of other sword-related specifics and I can thus not go into the
swords of the early Afghanistanis, Albanians, Algerians, ... (add 190 more member states of the UN), nor do I feel a necessity
to do so - except if I come across something of interest with regard to iron and steel
technology in this context. This applies to akinakes but not to Nimcha sabres. What I found out about akinakes is: an akinakes is a kind of double-edged straight dagger or short sword, made from bronze or iron. It was mainly used in the first millennium BC in the eastern Mediterranean region or Near East They are also connected to the Scythians and possibly to the Luristani stuff in some not-so-clear way. Now I'm interested. | ||
But not all that much. Most akinakes, it seems, are "found" in the
antiquities trade and that means four things:
|
||
| The point I'm trying to make is: This Hyperscipt is about Materials Science (you
must have noted that by now). It places special emphasize on iron and steel, including the history of these metals. Swords
are the paradigmatic embodiments of iron and steel, and that's what makes them interesting to me. I'm also interested in
many of the other aspects of swords but my priority is with
Materials Science. It follows that some arbitrary iron sword from the first millennium BC is of some interest to me - but not of much interest if I learn nothing about its metallurgy and how it was made. |
||
| Iron making in bulk did start in the East Mediterranean or Near East, and it is thus straight forward to assume that sword making also started in this region. The Luristani iron swords bear witness to this. That's why in this module I look a bit into the swords of the major powers that were present in this region in the first Millennium BC. However, when I looked more closely into the matter, it came to me as a surprise that only a few swords seem to be known from before 700 BC, say. Let's look at waht we have. | ||
| Akinakai | ||||||||||
| Here are some akinakai according to the description given by their sources. As you see, the come in bronze only, iron only, iron with bronze or gold hilts, and solid gold. You can classify them as short swords, dirks, or daggers. Take whatever pleases you; I don't care. | ||||||||||
| ||||||||||
| The gold betrays Scythian influence and dates the objects to 600 BC - 650 BC,
as stated by the Russian museum and fitting to the Scythian conquest of "the West"
including what's now Iran. The Medes were able to kick them out to some extent, while the Scythians were able to fend off
an invasion by Darius the Great of Persia's Achaemenid Empire in 513 BC. The Scythians are still rather mysterious, but
we do know that they were nomadic living people with horses, and that they had achieved an amazing mastery of gold metallurgy
if not metallurgy at large - just like the Luristanis. "Scythian
gold" is a well-known entity but they might also have mastered iron as shown be their very specail akenakai. That's why I decided to add a "Scythian Special" in 2020. |
| |||||||||
| The golden akinake is dated to the Achaemenid Empire, the first Persian empire founded by Cyrus
the Great, ca. 550 BC – 330 BC. There was a cultural interchange in other words (like plundering the
cities, killing the men, raping the women,..., as well as taking over the metallurgy knowledge) and that's probably how
Scythians skills made it to the Achaemenids. All these objects (except possibly the Russian one) come from illegal digging: Their historical value is thus limited. | ||||||||||
| ||||||||||
| The rusty thing above looks far less fetching than the pieces one
can buy. It is far superior, however: it was dug up by archaeologists in Persepolis, the
capital of the Achaemenid Empire. That allows us to conclude that around 500 BC somebody in the large Achaemenid Empire
knew how to forge a 65 cm long sword in one piece. That's almost impossible without fire welding. Unfortunately nothing else seems to be known about the iron /steel used for akinakes. We will have to wait. |
||||||||||
| The Scythians might have "invented " the akinake and used them as weapons
and as ceremonial objects. The other cultures, especially the Persians (and that includes
Luristan) adopted the design and akinakes became popular in the Mediterranean region and Near East. One might even see akinakes
as the forerunner of the Chinese "jinglu sword", the Greek xiphos,
and the Roman Gladius. Akinkakes were primarily a thrusting / stabbing weapon. I would tend to believe that they could not have been the main weapon for people living and fighting mostly on horse backs like the Scythians and Parthians. | ||||||||||
| Assyrian, Babylonian, Elamite, Achaemenid, and Parthian Swords | ||||||||||
| In the larger Eastern Mediterranean around 1200 BC iron gradually bcame a less
precious item (in some places) and appeared in larger quantities. However, what we have found so far, tends to be small
and relatively simple stuff. The "first" full iron
swords might be from from Luristan, a hard-to-get-to highland area of apparently no historic consequence then or ever.
Areas of consequence were empires or became parts of empires, like it or not. The important empires between 1200 BC and
roughly 250 BC are the ones relating to the names in the head line. In addition, we have the (usually not-so-innocent) bystanders
like the Scythians, Greeks, Egyptians, Cimmerians, Lydians, Phrygians, Luwians, Urarturians...., and, not to forget, the
Jews, Philistines, and so on. King David, one of the more unsavory characters of the Old Testament / Tanakh lived around
1000 BC - if he lived at all. It is a complex and possibly close to impossible undertaking to unravel exactly who made big progress in iron technology where and when. However, we may state with some reliability that major iron use, including the forging of complex objects did not take place before, roughly, the 8th century BC | ||||||||||
| All these names relate to the Eastern part of the Mediterranean or Near East.
On the West we had the Etruscians, Phoenicians, Romans, and so on. To the North we had the Celts (and some proto-Germanic
people). All of them (except the North, maybe) had some iron industry in the first millenium BC and, at the latest after
500 BC or so, made iron swords. I have already looked at the iron production in the "West" (Etruscans, Romans) and the North-West (Celts) after 500 BC. The question is what we know about the Assyrians, Babylonians, and so on. The answer is: Next to nothing. At least I couldn't easily find much that is worthwhile to be mentioned here. And I did spend some time in looking around. Just so you know what I'm talking about, I give you a quick list of the relevant empires with maps and a few facts in the link. |
| |||||||||
| Swords of the Assyrian Empire | ||||||||||
| The Assyrians ruled with the proverbial "iron fist", meaning that they
wielded iron weapons that were superior to the weapons of their opponents and that they were rather brutal in using their
iron. That they did have a large iron industry (or took over a large industry of vassal states) is proven by the huge hoard
of iron (160.000 kg!) found in the remains of the palace
in Khorsabad. Here is all I initially could find about Assyrian iron / steel weapons: |
||||||||||
| ||||||||||
| All I found besides the iron piece from the Khorsabad hoard is an old drawing depicting Assyrian weapons that somebody I don't know made some time ago, and an actual iron plate from some Assyrian armor. The Metropolitan Museum in NYC has many of these sorry things but nothing else the ancient Assyrians made from iron. | ||||||||||
| Well, several years later (it is now March 2020) I have to correct
that statement to some extent. I found 1. John Curtis' book: "An Examination of Late Assyrian Metal Work with Special Reference to Nimrud" (Oxford press, 2013). In this book many iron objects are shown and discussed. But it's typically iron spearheads, arrowheads, armor scales and other small stuff. There is a kind of large saw blade but there are still no (good) swords! All we have is the sorry lot shown here. One of the objects shows some similarity to what I have called the Luristan type 2 sword. 2. The article "IF I HAD KNOWN THAT MY LORD WANTED IRON. The beginning of the common use of iron in Assyria" from Caroline van der Brugge. Here is the link. The article is most illuminating and makes for good reading. Caroline argues that no iron ore is found in the Mesopotamian plane and that the Assyrians thus depended on others to supply iron or iron ore. She make a convincing case that large scale iron use in the Assyrian empire did not start before the end of the 8th century BC. |
||||||||||
| How do we know that Assyrian swords looked like the ones shown in the drawing?
From numerous large stone reliefs these guys left all over the place, in particular in Khorsabad. Here is Sargon II, fingering his sword (not necessarilly made from iron!) |
||||||||||
| ||||||||||
| However, these guys weren't just fondling their swords. They defeated about any other power around by then, the list is quite impressive. The following picture shows parts of the taking of a Mannean fortress in 715 BC, as depicted on a now lost relief from room 14 (slab 2) of Sargon II's palace at Khorsabad. Nobody has ever heard from the Manneam kingdom ever since. | ||||||||||
| ||||||||||
| However! There is some evidence that the Assyrians did not really use swords in
battle. Maybe the cavalry (if they has that) but not the infantry. The guys up their doing a sword fight actually use rather
short swords (akinakai?), if you look closely. Whenever the Assyrian (fighting) nobility became bored of killing people, they went out to kill some lions. With their sword! | ||||||||||
| ||||||||||
| There are many more picture like that, especially on seals. Those pictures makes me almost a liar. I wrote: "Even hunting animals with just a sword doesn't make much sense." Well. I do believe that even the most dedicated hunters out there today would be reluctant to hunt lions Assyrian style. Except, of course, the Romans. Sometimes they lost. But seriously now: You can't stop a charging lion like that. A grown lion weighs up to 820 pounds or 375 kg, the equivalent of 4 big people. Even if you manage to stab him as shown, he would throw you down quite forcefully and live long enough to take your head or damage you substantially in other ways. It is impossible for mere mortals - and thus only the king could do it as shown. | ||||||||||
What did we learn about Assyrian swords? Not much. Essentially we can only state:
| ||||||||||
| A bit more about Assyrians and their contemporaries can be found here | ||||||||||
| Swords of the Neo Babylonian Empire | ||||||||
| You are never too old to learn a new trick! Putting "babylon
sword" into Google, gives unexpected and possibly exciting results;
try it. Otherwise nothing. Nada | ||||||||
| Here is all I could find otherwise: | ||||||||
| ||||||||
| The two books going with the exhibition mentioned in the figure source contain
about 900 pages and more than 1000 pictures. The one above is the only one showing some iron. Maybe the Babylonian kings
didn't use a sword to demonstrate who Babylonian art, e.g. the famous pictures made from glazed tiles, does show soldiers but none with a sword. One relief showing a guy with a sword is assigned to Babylonians or Assyrians, depending on which source you read. So forget it. | ||||||||
| The end. Sorry. | ||||||||
| Swords of the Elamite Empire | ||||||||||||||
| We know the Elamites from way before as the makers of amazing silver and gold objects already around 3000 BC. Here is another example. One might assume that they must have been pretty good at bronze and iron, too. Bronze - yes. Iron - we don't know. Here is just one example for excellence with the three metals mentioned: | ||||||||||||||
| ||||||||||||||
The Elamite area is East of the Sumerians and Babylonians, containing mountainous
regions of what today is Iran. This map
gives a rough idea. The so-called proto Elamites who made the good stuff were around in 2700 BC. Even then they were having
constant fights with the powers down in the valley like the Sumerians; many of which they lost, leading to occupation and
so on. Just a few highlights.
|
||||||||||||||
| There is not much we have from the "iron age" Elamites. They appear rather in not-so-nice reliefs of the Assyrians: | ||||||||||||||
| ||||||||||||||
| I gave you all this because everything I have to say about Elamite swords you can find in this link! | ||||||||||||||
| Swords of the Achaemanid Empire | ||||||||
| Let's not waste time and space this time. Cyrus the Great conquered almost all there was to conquer (except the Greek), and he did that seemingly without swords. Even Khorasani's wonderful book doesn't offer a single picture and has very little to say. There seems to be one fries or whatever showing a guy with a long straight sword and one with a kind of kopis. If those things were made from bronze or iron is unknown | ||||||||
| In Persepolis, Cyrus' capital, we have many reliefs showing all kinds of people including soldiers. Almost none seems to be carrying a sword, Some preferred pretty handbags, it seems: | ||||||||
| ||||||||
| The exception is King Cyrus' weapon bearer who is shown on a large mural / frieze / relief, whatever you like to call that. Here is the important part: | ||||||||
| ||||||||
| Big deal. It's an akinake! Sorry - but that's it. We have no idea what Cyrus' smiths could do with iron. | ||||||||
| Swords of the Parthian Empire | ||||||||
| The Parthian Empire (247 BC – 224 AD) came about because one Arsaces I of Parthia, original a tribe chief, took the region of Parthia from the Seleucid Empire, the sequel to Alexander the Great's masterpiece. That's why it is also known as the Arsacid empire. King Mithridates I of Parthia (ca. 171 BC – 138 BC) greatly expanded the empire to what is shown here. The Parthians were essentially Persians and a clash with the Romans who were running a huge empire of their own by then, was unavoidable. | ||||||||
| Why do I mention Parthian swords here and not, for example, the "xiphos", the regular sword of the Greeks, swords from the empire of Alexander the Great, and so on. Because there is absolutely
nothing to learn about iron swords from these guys. We simply do not have many, if any.
In contrast to the Parthians! Here are Parthian iron swords: | ||||||||
| ||||||||
| Nothing to get very excited about. But at least those things were swords. The
left one was 67 cm long, the right one 87 cm. There is no big difference to the blades of the Celts or to any "Spatha"
between 500 BC and 1500 AD. It is hard to say but the blades appear to have neither a ridge nor a fuller, possibly just
the basic lenticular cross-section. No seams due to insufficient welding are visible, but also no indication of conscientious piling of different iron / steel grades. And of course there is no way of telling of these swords were hardened by quenching. There is also no way of telling if those sword are perhaps of Celtic origin. After all, my forebears were roaming the area already in 279 BC and even hung around for a few 100 years in Anatolia. |
||||||||
| So, sorry, but the Mediterranean and the Near East is a bit disappointing, sword-lore wise. It is time to move to the more exciting West and North - but not before a closing paragraph. | ||||||||
| Weird Swords | ||||||
| Museums own a lot of weird stuff. You just will not see it because it is usually
stored in the basement and locked up. Somebody sometime had dug up something weird, and it wasn't clear what it was or it
looked very unassuming. You can't throw it away, and you can't admit defeat either, so it goes into a box and into the basement.
And that's where it belongs because most of the time it is just random debris, indeed. But not always. Look up the "machine
of Antikythera", for example. It goes without saying that there many weird metal artifacts, including weird swords, had been dug up and confined to the basement | ||||||
| Khorasani, in his magnificent book, shows one weird sword. It is actually displayed in the Teheran Museum but nobody seems to have taken notice. Others turned up in auction catalogues. Here are a few: | ||||||
| ||||||
| The sword on the left, believed to come from Luristan, is 91 cm long. It looks like it has
a cast-on bronze hilt of a quite unusual shape since it has no pommel or lobes or other enlargements ensuring that the hand
doesn't slip. The Teheran sword was confiscated; its length is 104 cm; the blade alone measures 75 cm. What at a first glance looks like a long rusty tang is actually a cast-on slender bronze hilt that tapers to a point instead of of having a pommel of some kind. Its design and the way it is fixed to the blade seems to be unique. It is definitely very unusual. Both swords are of the "bi-metal" type with an iron blade and a bronze hilt. M;ore to those sword here. The "Hermann Historica" sword is described as: "Eisernes Griffzungenschwert" (Naue II), South-East Europe, 8th century BC. It is an exact copy of a bronze sword, a rather unusual thing. Here is a rather similar one. | ||||||
| Both swords have not been excavated so it is possible that they are fakes. It
is not likely however, because nobody in his right mind fakes unknown objects. What makes these two swords so special is
the fact that they seem to be the only long iron swords on (easily accessible) record for the first millennium BC in the
East Mediterranean / Middle East! That is quite remarkable, if you think about it. Could these swords be younger than 1000 BC? Well, yes - but they also could be older. There is just no way of knowing, short of doing a C14 analysis. | ||||||
| Could these swords be Celtic in origin? The Celts,
after all, did make it to Anatolia in 278 BC - as hired mercenaries. Even before that they were employed as fearsome warriors
by Mediterranean potentates. They did have their long swords then and earlier. Maybe a few made it to the East as booty
from some battle or as trade object. I do not think that this is a good explanation of the swords above but so far it seems to be the only one. | ||||||
| Constant warfare was a fact of life in the East Mediterranean / Middle East, just as about everywhere else. Why did we not find long swords in all the stuff dug up from about 1000 BC to 0 AD? The simplest explanation would be that there weren't many around. Depending on the fighting style, a long sword is not necessarily a good weapon. The Roman army, after all, did rather well for many centuries with the short gladius and the pilum (spear). Long swords or spathas were weapons for mounted warriors or crazy single-fighter egomaniacs like the Celts. | ||||||
| Long swords also make sense for executioners. From there it is a short way to long swords becoming symbols for power over life and death, a symbol
for the King. As a side benefit a normal King, not to mention a King
of the universe, looks so much better with a long heavily embellished sword (in addition to his gold
dagger or akinake) than with a short one. The hilts of the swords above make them not particularly fit for fighting. The balance without a pommel must be rather awful, and your grip could not have been very secure either. It is conceivable that they were only for representation, sort of highlights in the collection of strange war trophies. The hilt must have been added locally, and it is conceivable that is was made deliberately in a strange shape to emphasize the exotic nature of the sword. This is all wild guessing, of course. But more than that I cannot do. |
||||||
| There is a whole literature out there about long swords vs. short swords, and thrusting vs. slashing in fighting. Add fighting modes like single combat style to phalanx (closed ranks) style, fighting on horseback other mounted warriors or foot soldiers, and you can come up with endless lists of who should have had what and when. Add on top a certain amount of human stupidity, like fighting tanks on horseback because we are a cavalry unit after all, and everything is possible. The introduction of the metal shields, for example, might have changed fighting style from thrusting (short swords) to slashing (long sword or axe). Or maybe not. | ||||||
| Then it also matters to whom size matters. | ||||||
| 1) | JUSTYNA BARON and BEATA MIAZGA: "Scythian akinakes or medieval kidney-dagger? Archaeometric study of a recent find from Legnica (south-western Poland). Article in: Archaologisches Korrespondenzblatt · January 2013 |
© H. Föll (Iron, Steel and Swords script)