Semiconductor technology happens in factories. They need special materials, "reticles"
(= structures), "know-how" and huge amoundt of money (= capital) as major inputs |
|
|
|
 |
It's always about money! Only mass production will recover large investments. |
|
|
 |
The materials side always contains semiconductor substrates ("wafers") and often
very dangerous special "raw" materials. | |
|
 |
A number tells it all: 500 - 1.000 wafers /day are processed in a large Si "wafer
fab" | |
|
| |
| |
 |
Three big steps to Si wafers |
|
Sand (SiO2) Metallurgical Si Poly-Si |
Þ
Þ Þ |
Metallurgical Si
clean (doped) poly-Si. Single crystal / wafer |
|
|
 |
Si single crystal growth is done by "Czochralski process" (CZ). |
|
|
 |
Dislocation-free crystals are possible but "bulk microdefects" and impurities cannot
be totally avoided. | |
|
 |
Nearly perfect 300 mm wafers are standard. |
|
| |
|
|
© H. Föll (Semiconductor Technology - Script)