9. Real Steel

9.1 Some General Remarks

9.1.1 Things Get Complicated

9.1.2 Problems with Alloying

9.2 Low Alloy Steels

9.2.1 A Closer Look at Low Alloy Steels

9.2.2 Designing Low Alloy Steels

9.3 High Alloy steels

9.3.1 Stainless Steel

9.3.2 Maraging Steel

9.4 Phosphorous Steel

9.4.1 Phosphorous Steel - an Orderly Introduction

9.4.2 Phosphorous Steel - a Chaotic Succession

9.5 Cast-Iron

9.5.1 General Remarks

9.5.2 Kinds of Cast Iron