| Calculate numerical values for the mobility µ of some typical metals. | ||
| Take typical (metal) values for specific conductivity s and concentrations of electrons n and then calculate typical numbers for the mobility µ - do not take the values from the table! I you do not understand the German link, use this one. | ||
| Consider typical field strengths for metals by picking suitable current densities, and then derive typical values for the drift velocity vD. | ||
| Solution | ||
1.3.2 Ohms Law and Materials Properties