The equations for the concentration of the three point defects contain in parts the differnce of the formation enthalpies of Schottky or Frenkel defects. | |
| Calculate the ratio of the concentration of Schottky to Frenkel defects as a function of this enthalpy difference. | ||
| Discuss the result. Show in in particular, how large the difference must be if 90% or 99%, resp., of the defects are to be of one kind. | ||
| Link to the Solution | ||
Exercise 2.1-8 Quick Questions
Point Defects in Ionic Crystals
© H. Föll (Defects - Script)