| The following table contains some numbers found in the literature. for simple metals and Si. For more data activate the link | |||||||||||||||||||
| |||||||||||||||||||
2.1.1 Simple Vacancies and Interstitials
Values for the Formation Enthalpy of Vacancies
Exercise 2.1-6: Enthalpy difference for the limiting cases of Schottky or Frenkel Defects
© H. Föll (Defects - Script)