Optoelectronics has two basic branches: |
|
| | Wavelength (nm) | Typical Semiconductor |
| Infrared | 880 | GaAlAs/GaAs | | Red |
660 - 633 | GaAlAs/GaAs | Orange to Yellow |
612 - 585 | AlGaInP GaAsP/GaP GaAsP/GaP |
| Green | 555 | GaP | Blue to
Ultraviolet | 470 - 395 | GaN/SiC GaN/SiC InGaN/SiC |
|
|
 |
1. Light in Þ electrical signal out:
| |
|
|
- Optical sensors as single elements
- "CCD" chips in "megapixel" matrices.
|
|
|
 |
2. Electricity in Þ light out; in two paradigmatic versions:
| |
|
| | |
 |
Here we only look at the second branch. |
|
|
 |
The semiconductors of choice are mostly the III-V's, usually in single-crystalline perfect thin films.
| |
|
 |
The present day (2008) range of wavelength covers the IR to near UV. |
|
|
 |
Indirect semiconductors like GaP can be used too, if some "tricks" are used. |
|
| |
| |
|
 |
The index of refraction
n=(e)½ and thus the dielectric constant e
become important | |
Typical Semiconductor |
Dielectric constant |
Thermal conductivity [W/cm · K] |
| Si | 11.9 | 1.5 | | GaAs |
13.1 | 0,45 | | GaP | 11.1 | 1.1 |
| GaN | 8.9 | 1.3 | | SiC |
10 | 5 | | C (Diamond) |
5.8 | 22 |
|
|
 |
Semiconductors have a relatively large index of refraction at photon energies below the bandgap
of n » 3 - 4. | |
|
 |
Diamond has the highest n in the visible region |
|
 |
The thermal conductivity becomes important
because for generating light one needs power (which we avoided as much as possible for
signal processing with Si!) | |
|
 |
Again, diamond has the highest thermal conductivity of all known materials - 5 times
better than Cu! | |
| | |
| |
 |
LED's come as cheap little "indicator" lights and recently also
as replacement for "light bulbs". | |
|
|
 |
Intense white light from LED's becomes possible, Advantages: High efficiencies and
long life time | |
|
 |
The key was the "taming" of the GaN material system for blue and UV LED's. |
|
 |
LED's based on organic semiconductors (OLED) are rapidly appearing
in OLED based displays. | |
|
 |
Advantage: High efficiencies because of active light generation.
Problem: Product life time; sensitivity to air. |
|
| |
| |
|
 |
Semiconductor "Diode" Lasers are high-power" LED's
plus "mirrors" | |
Enabling technology for CD / DVD / Blue ray / ... memory technologies! |
|
|
 |
Advantage: Small and cheap.
Problems: Low power, "Quality". |
|
| |
| |
|