| The picture, once more taken from "Read and Hull", shows the dislocation reactions and movements leading to the formation of a stacking fault tetrahedra in the short-hand notation of the Thompson tetrahedra. | |||
| |||
5.4.3 Some Details for Specific Lattices
© H. Föll (Defects - Script)