| Suffice it to say that now (2019) SiC is finally taking off. The Bosch company is heavily investing in SiC devices for handling power, presumably inside the "electric" car (and in trains, of course). | ||
|
|
We also see SiC in the power modules handling solar power and in the ultra-high speed power modules needed for the "G5" technology in communications. | |