The name, obviously, has nothing to do with "Ferro"
(= Iron), but associates the analogy to ferro magnetism. It means that in some special materials, the electrical dipoles
are not randomly distributed, but interact in such a way as to align themselves even
without an external field. |
|
 |
We thus expect spontaneous polarization and a very large dielectric constant (DK). |
|
 |
This should be very useful - e.g. for making capacitors - but as in the case of ferro magnetism,
there are not too many materials showing this behavior. |
 |
The best known material used for many application is BaTiO3 (Barium titanate). |
|
 |
It has a simple lattice as far as materials with three different atoms can have a simple lattice at all.
The doubly charged Ba2+ atoms sits on the corners of a cube, the O2– ions on the
face centers, and the Ti4+ ion in the center of the cube. |
|
 |
We have 8 Ba2+ ions belonging to 1/8 to the elementary cell, 6 O2–
ions belonging to 1/2 to the elementary cell, and one Ti4+ ion belonging in total to the cell,
which gives us the BaTiO3 stoichiometry. |
|
 |
This kind of crystal structure is called a Perovskite structure;
it is very common in nature and looks like the drawing below (only three of the six oxygen ions are shown for clarity): |
| |
|
|
Often, the lattice is not exactly cubic, but slightly distorted. In the case of
BaTiO3 this is indeed the case: The Ti - ion does not sit in the exact
center of the slightly distorted cube, but slightly off to one side. It thus has two
symmetrical positions as schematically (and much exaggeratedly) shown below |
|
|
|
 |
Each elementary cell of BaTiO3 thus carries a dipole moment, and, what's
more important, the moments of neighbouring cells tend to line up. |
 |
The interactions between the dipoles that lead to a line-up can only be understood with quantum
mechanics. It is not unlike the interactions of spins that lead to ferro magnetism. |
|
 |
We will not go into details of ferro electricity at this point. Suffice it to say that there
are many uses. Traditionally, many capacitors use ferro-electric materials with high DK values. In recent years,
a large interest in ferro-electrics for uses in integrated circuits has developed; we have yet to see if this will turn
into new products. |
| | |
|