Do the Math

Solve the system of the three equations given below and show that the result given is correct
 
cV · ci = N´/N · exp-hFP/kT
 
 
What are the conditions for the limiting cases of pure Frenekel or Schottky defects?
 

Link to theSolution


gehe zu 2.2.2 Gemischte Fehlordnung