Cross-Sectional TEM of Si - NiSi
2
Interfaces
Shown are two cross-section of the
Si - NiSi
2
interface (and the
NiSi
2
surface).
Facetting
of the interface on
{111}
is very prominent, but the
NiSi
2
surface shows facets, too..