| The following sequence of pictures (taken from "Read and Hull") shows the formation of a Lomer-Cotrell dislocation. | |||
| Two perfect dislocations on different {111} planes split into Shockley partials, move until they meet, and react. The end end product of the reaction is a stair-rod dislocation with a Lomer-Cotrell dislocation at its apex. | |||
| |||