| Shown is the force between edge dislocations of identical and opposite Burgers vectors as a function of their normalized distance. | |||
| The distance x between the dislocations is expressed in units of y, the distance of the glide planes. | |||
| The force changes from repulsive to attractive or vice verse for a distance x = y; i.e. if the dislocations are at an angle of 45o relative to the glide plane. | |||
| The 45o position is a stable equilibrium position for opposite Burgers vectors, because at this position F = 0, and dF/dx < 0. | |||
| For dislocations with identical b vectors, the stable position is at x = 0. | |||
| |||
5.2.5 Interactions Between Dislocations
© H. Föll (Defects - Script)