Overview of Heating Materials
|
The diagram shows the temperature range and the resistivity of typical materials
for heating elements. |
|
 |
Do not forget that humble 1500 oC (roughly the melting point
of iron) means that it is really hot! Mankind had to invent pretty tricky crafts for
about 2000 years because nobody could reach the
melting point of iron. |
|
 |
Beyond 2000 oC there are not many usable materials left. Essentially you
are stuck with graphite (not in the figure). |
|
|
| |
|
With frame

2.3.3 Resistors and Heating
© H. Föll (Advanced Materials B, part 1 - script)