| Here are a few diagrams showing the energy levels of dopants and some other impurities in the band gap of III-V compound semiconductors | |||
| For the time being, only GaAs data are presented. | |||
| |||
5.1.3 Doping of Compound Semiconductors
© H. Föll (Semiconductors - Script)