| Here is the complex index of referaction of Silicon (from Handbook of Optical Constants of Solids (E.D. Palik)) | |||
| |||
| Note that the imaginary part k increases as soon as the wavelength is small enough for band-to-band absorption processes; i.e. h · n > EG applied (with EG = band gap). | |||
3.7.2 The Complex Index of Refraction
© H. Föll (Electronic Materials - Script)