Some Properties of Cu Alloys
The following table lists just a few of the existing
Cu
based alloys for specific uses.
Alloy
Essential
Advantage
s
10
4
S/cm
1)
Uses
Cu + 0,2% Ag
relatively hard
57
Collector lamellae
Cu + 0,5% Te
easy machinable
55
precision parts
Cu + 1,2% Cd
high strength
52
Overhead wires for trains
Cu + 0,6% Cr
can be hardened
48
Welding electrodes
Cu + 1,7% Be
can be hardened
18
Contact springs
1)
S = Siemens = 1/
W
With frame
2.2.1 General Applications
© H. Föll (Electronic Materials - Script)