| The figure shows some materials for heating elements and the maximal temperature they can endure. | |||
| Note that the maximum temperature, while more or less scaling with the melting point, is usually well below the melting point - because most materials start to develop all kinds of problems long before they melt. | |||
| |||
© H. Föll (Advanced Materials B, part 1 - script)