| Here is a plot of the specific resistivity vs. temperature for some metals. | |||
| The resistivity seems to go to 0 for 0 K. This is not really true, cf. the detailed curve for Na. | |||
| Still, simple free electron theory predicts zero resistance at 0 K, and trying to see if that is true was one of the driving forces behind the discovery of superconductivity by Kammerlingh Onnes in 1911. | |||
| |||